Thermally prepared mixed-oxide IrO2+ZrO2 films were studied by Rutherford backscattering spectrometry (RBS), wide-angle x-ray scattering (WAXS) and cyclic voltammetry. Concentration depth profiling by RBS has shown that electrode films containing <50 mol.% of IrO2 have layered structures where noble metal oxide and ZrO2 enrichments alternate. The outermost layer is enriched with IrO2. By WAXS analysis it was possible to prove the existence of an IrO2 and a ZrO2 phase. From cell parameters, very limited solubility could be ascertained, restricted at the 2 limits of the composition coordinate. In the range 0-20 mol.% of IrO2, a tetragonal ZrO2 phase is formed. For samples richer in IrO2, the ZrO2 phase becomes amorphous. The microstructural features of the tetragonal IrO2-rich phase do not change significantly with the film composition. The effective surface area of the samples, as determined by cyclic voltammetry, exhibits a maximum in the composition range 50-80 mol.% IrO2. This result was interpreted on the basis of WAXS and RBS data.

Physicochemical properties of thermally prepared Ti-supported IrO2+ ZrO2 electrocatalysts

DE BATTISTI, Achille;
1994

Abstract

Thermally prepared mixed-oxide IrO2+ZrO2 films were studied by Rutherford backscattering spectrometry (RBS), wide-angle x-ray scattering (WAXS) and cyclic voltammetry. Concentration depth profiling by RBS has shown that electrode films containing <50 mol.% of IrO2 have layered structures where noble metal oxide and ZrO2 enrichments alternate. The outermost layer is enriched with IrO2. By WAXS analysis it was possible to prove the existence of an IrO2 and a ZrO2 phase. From cell parameters, very limited solubility could be ascertained, restricted at the 2 limits of the composition coordinate. In the range 0-20 mol.% of IrO2, a tetragonal ZrO2 phase is formed. For samples richer in IrO2, the ZrO2 phase becomes amorphous. The microstructural features of the tetragonal IrO2-rich phase do not change significantly with the film composition. The effective surface area of the samples, as determined by cyclic voltammetry, exhibits a maximum in the composition range 50-80 mol.% IrO2. This result was interpreted on the basis of WAXS and RBS data.
1994
DE BATTISTI, Achille; Benedetti, A.; Riello, P.; Battaglin, G.; Barbieri, A.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in SFERA sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11392/461089
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 46
  • ???jsp.display-item.citation.isi??? 43
social impact