A safe lithium-sulfur (Li−S) battery employs a composite polymer electrolyte based on a poly(ethylene glycol) dimethyl ether (PEGDME) solid at room temperature. The electrolyte membrane enables a stable and reversible Li−S electrochemical process already at 50 °C, with low resistance at the electrode/electrolyte interphase and fast Li+ transport. The relatively low molecular weight of the PEGDME and the optimal membrane composition in terms of salts and ceramic allow a liquid-like Li−S conversion reaction by heating at moderately high temperature, still holding the solid-like polymer state of the cell. Therefore, the electrochemical reaction of the polymer Li−S cell is characterized by the typical dissolution of lithium polysulfides into the electrolyte medium during discharge and the subsequent deposition of sulfur at the electrode/electrolyte interphase during charge. On the other hand, the remarkable thermal stability of the composite polymer electrolyte (up to 300 °C) suggests a lithium-metal battery with safety content significantly higher than that using the common, flammable liquid solutions. Hence, the Li−S polymer battery delivers at 50 °C and 2 V a stable capacity approaching 700 mAh gS−1, with a steady-state coulombic efficiency of 98 %. These results suggest a novel, alternative approach to achieve safe, high-energy batteries with solid polymer configuration.

Novel Lithium-Sulfur Polymer Battery Operating at Moderate Temperature

Marangon V.
Primo
;
Hassoun J.
Ultimo
2021

Abstract

A safe lithium-sulfur (Li−S) battery employs a composite polymer electrolyte based on a poly(ethylene glycol) dimethyl ether (PEGDME) solid at room temperature. The electrolyte membrane enables a stable and reversible Li−S electrochemical process already at 50 °C, with low resistance at the electrode/electrolyte interphase and fast Li+ transport. The relatively low molecular weight of the PEGDME and the optimal membrane composition in terms of salts and ceramic allow a liquid-like Li−S conversion reaction by heating at moderately high temperature, still holding the solid-like polymer state of the cell. Therefore, the electrochemical reaction of the polymer Li−S cell is characterized by the typical dissolution of lithium polysulfides into the electrolyte medium during discharge and the subsequent deposition of sulfur at the electrode/electrolyte interphase during charge. On the other hand, the remarkable thermal stability of the composite polymer electrolyte (up to 300 °C) suggests a lithium-metal battery with safety content significantly higher than that using the common, flammable liquid solutions. Hence, the Li−S polymer battery delivers at 50 °C and 2 V a stable capacity approaching 700 mAh gS−1, with a steady-state coulombic efficiency of 98 %. These results suggest a novel, alternative approach to achieve safe, high-energy batteries with solid polymer configuration.
2021
Marangon, V.; Di Lecce, D.; Minnetti, L.; Hassoun, J.
File in questo prodotto:
File Dimensione Formato  
ChemElectroChem - 2021 - Marangon - Novel Lithium‐Sulfur Polymer Battery Operating at Moderate Temperature.pdf

accesso aperto

Descrizione: Full text editoriale
Tipologia: Full text (versione editoriale)
Licenza: Creative commons
Dimensione 4.64 MB
Formato Adobe PDF
4.64 MB Adobe PDF Visualizza/Apri

I documenti in SFERA sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11392/2467407
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 11
  • ???jsp.display-item.citation.isi??? 11
social impact